Sigh! It helps to get the story right. The missing word here is oxidation. Many semiconductor processes are conducted in vacuum or in low-pressure atmospheres of, for example hydrogen. In this case, storing the Copper Indium Selenide in a nitrogen atmosphere before passivation with Cadnium Sulfide or whatever, should allow storage for weeks, but would usually be minutes to hours in a typical fab.